Spring Grade 52cr4mo2v Chemical

Download as pdf or txt
Download as pdf or txt
You are on page 1of 1

8/20/2015 ISMT 

| Comparison of Different Steel Compositions for Commonly Used Steel Grades at ISMT

Company Profile Product & Services Infrastructure Investor Relations Quality Newsroom Careers @ ISMT

Steel Grade Comparison Chart
Back to Steel Grade Home 

Comparison of Different Steel Compositions for Commonly Used Steel Grades at ISMT

  52Cr4Mo2V SCM 22 H/SCM 420H SCM 430

Carbon (C) 0.48­0.56  0.18­0.23  0.28­0.33 

Manganese (Mn) 0.70­1.10  0.60­0.85  0.60­0.85 

Silicon (Si) 0.15­0.40  0.15­0.35  0.15­0.35 

Sulphur (S) 0.02 Max  0.01 Max  0.03 Max 

Phosphorus (P) 0.02 Max  0.02 Max  0.03 Max 

Nickel (Ni) 0.30 Max  0.20 Max  0.30 Max 

Chromium (Cr) 0.90­1.20  0.90­1.20  0.90­1.20 

Molybdanum (Mo) 0.15­0.25  0.15­0.30  0.15­0.30 

Vanadium (V) 0.07­0.12  0.02 Max  0.03 Max 

Titanium (Ti) 0.03 Max  0.02 Max  0.03 Max 

Aluminium (Al) 0.06 Max  0.02­0.04  0.06 Max 

Cupper (Cu) 0.30 Max  0.20 Max  0.30 Max 

Tin (Sn) 0.02 Max  0.01 Max  0.02 Max 

Oxygen (O2)   20.00 ppm Max   

Y.S.      

UTS   95.00 Min   

%E   14.00 Min   
 
Foot Note: Please contact ISMT for customization of your requirements. Contact: [email protected]